Conversion Coating Pretreatment Enhances Pipeline Integrity
[1]
Makanjuola Oki, Department of Mechanical Engineering, Landmark University, Omu-Aran, Kwara State, Nigeria.
[2]
Adeolu Adesoji Adediran, Department of Mechanical Engineering, Landmark University, Omu-Aran, Kwara State, Nigeria; Department of Mechanical Engineering Science, University of Johannesburg, Johannesburg, South Africa.
[3]
Bamidele Ogunsemi, Department of Mechanical Engineering, Landmark University, Omu-Aran, Kwara State, Nigeria.
[4]
Sarah Abidemi Akintola, Department of Petroleum Engineering, University of Ibadan, Ibadan, Oyo State, Nigeria.
[5]
Ebitei Charles, Department of Mechanical Engineering, Niger Delta University, Bayelsa State, Nigeria.
It is necessary to coat both the internal and external surfaces of pipelines which transport different types of fluids that are usually contaminated with various percentages of aggressive corrosives. Pipelines pass through various terrains and highly challenging environments hence the need for both internal and external coatings to prevent corrosion and its adverse effects. In order to improve on the longevity of pipelines and the adhesion of the coating system, it is preferable to conversion coat blasted surfaces prior to application of any coating system. Improvements in pipeline coatings applications and the often neglected chromating procedure prior to coating application have been highlighted. This will prolong the lifespan of pipeline networks and secure these strategic assets from being a source of both materials and human resources drain pipes. However, the use of corrosion resistant alloys as internal lining for carbon steel pipes in the petroleum/gas industry is fast gaining recognition.
Oil/Gas Industry, Conversion Coating, Pipeline, Corrosion
[1]
Thomson, G. E (1994) “Conversion coatings” TALAT Lecture series 5202, European Aluminium Association, (1994) pp. 1-9.
[2]
Oki, M “Functionalised chromate conversion coating” Nigerian Patent NG/P/2013/755, April, 2014.
[3]
Bates, C Pyrene chemicals UK, Industrial corrosion (1988) C7-C8.
[4]
Chen, T, Chen, R, Jin, Z and Liu, J “Engineering hollow mesoporous silica nano-containers with molecular switches for continuous self-healing anticorrosion coating” Journal of Materials Chemistry A. 3 (2015) 9510-9516. DOI: 10.1039/c5ta01188d.
[5]
Khramov, A. N, Voevodin, N. N, Balbyshev, V. N. and Donley, M. S. “Hybrid organo-ceramic corrosion protection coatings with encapsulated organic corrosion inhibitors” Thin Solid Films 447-448 (2004) 549–557.
[6]
Zheludkevich, M. L., Shchukin, D. G., Yasakau, M¨ohwald, H and Ferreira, M. G. S “Anticorrosion coatings with self-healing effect based on nano-containers impregnated with corrosion inhibitor” Chemistry of Materials 19 (3) (2007) 402–411.
[7]
Khramov, A. N, Voevodin, N. N, Balbyshev, V. N and Mantz, R. A, “Sol–gel-derived corrosion-protective coatings with controllable release of incorporated organic corrosion inhibitors” Thin Solid Films 483 (1–2) (2005) 191–196.
[8]
Rajendran, R. J, Rathish, S. S. Prabha “Self-assembling nano films on metal surface as corrosion inhibitors” Advanced Materials Proceedings 2 (9) (2017) 596-601.
[9]
Izadi. M, Shahrabi, T, and Ramezanzadeh, B “Electrochemical investigations of the corrosion resistance of a hybrid sol–gel film containing green corrosion inhibitor-encapsulated nano-containers” Journal of the Taiwan Institute of Chemical Engineers 81 (2017) 356–372.
[10]
Ramezanzadeh, B, Akbarian, M, Ramezanzadeh, M., Mahdavian, M, Alibakhshi, E and Kardar, P “Corrosion protection of steel with zinc phosphate conversion coating and post-treatment by hybrid organic-inorganic sol-gel based silane film” J. Electrochem. Soc. 164 (6) (2017) C224–C230.
[11]
“https://www.epa.gov/indoor-air-quality-iaq/volatile-organic-compounds-impact-indoor-air-quality” accessed on 7/25/2017 at 1600hrs.
[12]
M. Oki “Studies on chromium-free conversion coatings on aluminium” Journal of Applied Science and Environmental Management 11 (2) (2007) 187-190.
[13]
C. A. Matzdorf, W. C. Nickerson, E. Lipnickas “Evaluation of modified zirconium/trivalent chromium conversion coatings by accelerated corrosion and electrochemical techniques” Tri-service corrosion conference, 2005.
[14]
C. A. Matzdorf, W. C. Nickerson Patent No. 0230215. USA 2003.
[15]
T. G. Harvey “Cerium-based conversion coatings on aluminium alloys: a process review” Corros. Eng. Sci. Technol., 48, (2013) 248–269.
[16]
C. G. da Silva, C. P. Margarit-Mattos, O. R. Mattos, H. Perrot, B. Tribollet, V. Vivier “The molybdate–zinc conversion process” Corrosion Science 51 (2009) 151–158.
[17]
M. Oki, A. A. Adediran, S. Olayinka, O. Ogunsola “Development and performance of hybrid coatings on aluminium alloy” J. Electrochem. Sci. Eng. 7 (3) (2017) 131-138; DOI: http://dx.doi.org/10.5599/jese.347.
[18]
M. W. Kendig and R. G. Buchheit “Corrosion inhibition of aluminum and aluminum alloys by soluble chromates, chromate coatings, and chromate-free coatings” Corrosion 59 (2003) 379–400.
[19]
M. Oki “Functionalised chromate conversion coating” Patent number, NG/P/2013/755, April, 2014.
[20]
M. Izadi, T. Shahrabi, B. Ramezanzadeh “Electrochemical investigations of the corrosion resistance of a hybrid sol–gel film containing green corrosion inhibitor-encapsulated nano-containers” Journal of the Taiwan Institute of Chemical Engineers 81 (2017) 356–372.